Hypertherm Accepting Applications for its Spark Something Great Educational Grant

Hypertherm, Hanover, N.H., a manufacturer of industrial cutting systems and software, is accepting applications for its Spark Something Great educational grant program.

AWS Publications | February 25, 2021 | Tech and Industries
Welding Digest ►  Hypertherm Accepting Applications for its Spark Something Great Educational Grant

Hypertherm, Hanover, N.H., a manufacturer of industrial cutting systems and software, is accepting applications for its Spark Something Great educational grant program.

In total, the company plans to award a Powermax45® XP plasma system and deliver in-person training to 12 North American schools (Figure 1).  

The Spark Something Great grant program is now in its seventh year. The grant is meant to support the next generation of welders and metal fabricators by making the newest generation of plasma cutting equipment and standardized instruction available to schools. To date, the company has awarded systems to 64 schools.   

In addition to the grant program, the company will continue to make all ten hours of its AWS SENSE approved Plasma Cutting Technology: Theory and Practice curriculum available for free download to teachers. The curriculum covers the plasma cutting process, common industrial uses for plasma systems, the differences between various cutting methods, safety procedures as well as proper setup and operation. Electronic versions of each lesson, a facilitator’s guide, student workbook, and supporting reference material are all available at hypertherm.com/plasmaeducation.  

“Although many programs are limited to online instruction only because of the pandemic, we want to ensure teachers have the resources they need to make up lost ground once students return to the classroom,” said Betsy Van Duyne, who manages Hypertherm’s educational program. “This grant will provide 12 schools with a highly capable system, giving teachers the flexibility to teach both handheld and mechanized cutting, as well as applications such as gouging, flush cutting and marking with air plasma.”  

Applications for the Spark Something Great grant are due on or before April 2 with grant decisions communicated by May 3. For more information, including instructions for applying, go to hypertherm.com/grant 

Figure 1-Feb-25-2021-05-42-31-13-PM

Figure 1: Hypertherm’s 2021 Spark Something Great education grant program will award 12 North American schools with a Powermax45 XP and in-person training. The application process is open now and closes April 2.